and not by the tool itself. This causes an erosion and the subsequent rupture of the tip. The breaking in these cases usually appears at the top of the hammer pin as a result of the idle strokes when the tip of the tool / GK 950 960 is
and not by the tool itself. This causes an erosion and the subsequent rupture of the tip. The breaking in these cases usually appears at the top of the hammer pin as a result of the idle strokes when the tip of the tool / GK 950 960 is
or light 950 GK / 960 materials are called idle strokes. This happens when the piston does not stroke the hammer tool, and the impact force and energy is absorbed by bolts and the tool retaining screws and not by the tool itself. This causes an erosion and the subsequent rupture of the tip. The
LOW TEMPERATURES At low temperatures it is recommended that the tools be heated before use and if / 950 GK 960 it is possible use at low speed for a progressive increase in temperature of the machinery.