DO NOT EXECUTE IDLE STROKES
and energy is absorbed by bolts and the tool retaining screws and not by the tool itself. This causes an erosion ALG 160 HF 32 - and the subsequent rupture of the tip. The breaking in these cases usually appears at the top of the hammer pin as a result of the idle strokes when the tip of the tool
LOW TEMPERATURES
LOW TEMPERATURES At low temperatures it is recommended - ALG 160 32 HF that the tools be heated before use and if it is possible use at low speed for a progressive increase in temperature of the machinery.
CONSTANT LUBIRICATION
CONSTANT ALG HF 32 160 - LUBIRICATION Even if the hammer is provided with a lubrication system, it is necessary to lubricate the tip of the tool to avoid the friction between metals.